Microstructured fiber splicing
Concerning the spreading results, the reproducibility of the electric arcs as well as the quality of the cleaves from one ... Results are presented in Fig. 3. Fusion losses are generally grouped between 0.7 and 1.1 dB for arc durations of 0.40 or 0.45 ... The results of various fusions are presented in Fig. 6. We first noticed that very low-loss fusions of two MOFs were possible ... The results presented in Fig. 3 indicate a breaking force varying between 20 and 80 kpsi. To give us a reference value, we ...